The phenolic foam roof insulation turned out to have a critical flaw.
Phenolic foam roofing insulation problems.
Hundreds of millions of square feet of phenolic foam produced in oak creek were installed on structures nationwide between 1981 and 1992 according to the companies.
Beazer phenolic foam roof insulation was manufactured and shipped from 1980 through january 1989 for use as roof insulation.
Because a number of commercial roofing companies have installed this roof system poorly or incorrectly this misnomer is one of the greater misperceptions to emerge in the commercial roofing industry.
It alleges that the phenolic foam roof insulation applied to two east coast buildings corroded the underlying steel deck and other metal components.
Continual improvements in the formulations of phenolic foam board insulation products may overcome these drawbacks.
Pinhole or pitting corrosion problems are common with copper pipes steel water pipes and stainless steel steam pipes when insulated with phenolic foam and the pipework gets wet.
When it was installed over a lightly primed painted metal deck any water in the roof system from above moisture from operations or humidity within the building activated chemicals in the phenolic foam which caused corrosion of the metal deck.
Spray polyurethane foam technology does not have a solid track record for commercial roofing.
Phenolic insulation exposed to humidity or direct moisture such as roof leaking creates sulphonic acid.
Beazer pfri has been the subject of a putative class action lawsuit in which the plaintiffs allege that beazer pfri causes severe corrosion to metal roof decks and other damage to roofing systems.
Briefly a phenolic foam remediation project demands these steps.
Spray foam roofing problems and myths answered.
In the 1980s and sold by beazer east and johns manville but serious corrosion problems resulted in legal action and both companies ceased production in 1992.
The main problems with phenolic foams reported in the 1980 s were their relatively low compressive and flexural strength and their friability or tendency to crumble.
Removal of existing roofing materials and insulation down to the deck.
Only a day s worth of work should be undertaken to avoid leaving the building vulnerable to the elements.
Phenolic foam insulation is known to shrink after curing placement in the walls of your home or between.
The risks of phenolic foam insulation shrinkage.
Phenolic foam rigid insulation was introduced in the u s.